ER4043 5LB Aluminum TIG Welding Rod
ER4043-5LB-1-6
- Free Contiguous US Shipping Over $150
- In stock, ready to ship
- Inventory on the way
Welding Wire ER4043 can use where base metal requires thermal treatment. It also can be used on weld forge and casting materials.
Commonly referred to as “AlSi5", has a 5% silicon. It contains silicon additions, improving the weld pool's fluidity and making the welding less sensitive to cracking. The bright finish is a good choice for welders
Most widely used as filler metal ER4043 rod for TIG welding (GTAW) welding process in aluminum welding for general purpose applications.
Usually 100% Argon, Helium, or mix.
It can weld various grades of aluminum, 3003, 3004, 5052, 6061, 6063, and casing alloys 43, 355, 356, and 214.
Available diameters: 1/16", 3/32" in length. Package of 5-Lb.
Note: YesWelder welding rods are shorter than other brands' welding rods.
WARNING: This product can expose you to chemicals known to the State of California to cause cancer and birth defects or other reproductive harm. For more information, visit www.P65Warnings.ca.gov.
Most items are usually shipped within 3-5 working days. Your delivery confirmation email will contain your tracking number and order details. Should you have any questions, our team is also on hand 7 days a week and can be reached at support@yeswelder.com.