Banner Image

DESCRIPTION

The YesWelder MIG-205DS offers multiprocess welding, MIG, TIG, and Stick (Arc), with inverter technology. This dual voltage mahcine will go up to 160 Amps at 110V, and up. to 205 Amps at 220V (60% duty cycle each). Use the synergic mode. for easy settings, or control the Amps and Volts manually. You. can even change the inductance.

FEATURES

  • Synergic Controlled on MIG function, very easy and simple operation.
  • 4 Functions in 1 of Gas MIG /Gasless MIG / Lift TIG / Stick
  • Can take up to 0.9mm(.035") MIG solid wire(Gas MIG) and 0.9mm(.035") MIG FLux wire(Gasless MIG)
  • Only Apply to D100 / D200 rolls (4โ€ / 8โ€ diamater rolls๏ผ‰(<10lbs) of MIG wire
  • 200 Amp Gas/Gasless MIG welder with a 50 Amp plug(220V)
  • 160 Amp Gas/Gasless MIG welder with a 35 Amp plug(110V)