ER70S-6-1.6 TIG welding rod
ER70S-6-2.4 TIG welding rod
ER70S-6-5LB Mild  Steel TIG Welding Rod - YesWelder
1.6mmStainless Steel TIG Welding Rod
Stainless Steel TIG Welding Electrode
ER308L 5LB Stainless Steel TIG Welding Rod

ER70S-6 and ER308L TIG Filler Rods

ER70S-6-5LB-1-6

Regular price39.00
/
Diameter
Filler Metal
Weight
  • Free Contiguous US Shipping Over $150
  • In stock, ready to ship
  • Inventory on the way

ER70S-6 is intended for mild and carbon steel, while ER308L is a low-carbon filler for compatible stainless steels such as 304/304L. Both support TIG fabrication and repair work.

Choose the Right Filler Metal

ER70S-6 Mild Steel: For TIG welding mild and carbon steel in structural fabrication, automotive repair, farm equipment, tanks, and general repair work.

ER308L Stainless Steel: A low-carbon stainless filler for compatible 304/304L, 308, and 321 stainless steel used in fabrication, equipment, tanks, and piping.

Key Specifications

  • Filler metal options: ER70S-6 Mild Steel and ER308L Stainless Steel
  • Process: TIG
  • Package weight: 5 lb (2.3 kg)
  • Rod length: 16" (400 mm)
  • Diameter options: 1/16" (1.6 mm), 3/32" (2.4 mm), and 1/8" (3.2 mm)
  • Shielding gas: 100% Argon or an Argon / Helium mixture

WARNING: This product can expose you to chemicals known to the State of California to cause cancer and birth defects or other reproductive harm. For more information, visit www.P65Warnings.ca.gov.