Carbon Steel MIG Solid Welding Wire,ER70S-6 .035-Inch on 10-Pound Spool
Carbon Steel MIG Solid Welding Wire,ER70S-6 .035-Inch on 10-Pound Spool
ER70S-6/10LB-0.9 .035" 10LB Spool Carbon Steel Solid MIG Welding Wire
3 Pieces 10LB Spool Carbon Steel Solid MIG Welding Wire
5 Pieces 10LB Spool Carbon Steel Solid MIG Welding Wire
ER70S-6/10LB-0.9 .035" 10LB Spool Carbon Steel Solid MIG Welding Wire Hardware > Tool Accessories > Welding Wire YesWelder 2PKS
ER70S-6/10LB 10LB Spool Carbon Steel Solid MIG Welding Wire - YesWelder
ER70S-6/10LB-0.8 .030" 10LB Spool Carbon Steel Solid MIG Welding Wire Hardware > Tool Accessories > Welding Wire YesWelder 2 PKS
5 Pieces 10LB Spool Carbon Steel Solid MIG Welding Wire

ER70S-6/10LB 10LB Spool Carbon Steel Solid MIG Welding Wire

ER70S-6/10LB-0.9

Sale price42.00
/
Quantity
Diameter
  • Free Contiguous US Shipping Over $150
  • In stock, ready to ship
  • Inventory on the way

  • ER70S-6 has the highest combination of manganese and silicon deoxidizers, permitting higher welding currents with 100% CO2 shielding gas and leaving a smoother weld bead with little to zero post-weld cleanup.
  • ER70S-6 is the most common of the copper-coated mild steel GMAW (MIG) wires for single or multiple pass welding
  • Great for construction work, farm implement fabrication, shaft buildup, tanks, truck bodies and general shop applications with poor fit-up or rusty, oily plates.
  • 10-Pound spool

WARNING: This product can expose you to chemicals known to the State of California to cause cancer and birth defects or other reproductive harm. For more information, visit www.P65Warnings.ca.gov.

Most items are usually shipped within 3-5 working days.ย Your delivery confirmation email will contain your tracking number and order details.ย Should you have any questions, our team is also on hand 7 days a week and can be reached at support@yeswelder.com.

This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.