The jacket uses 11 oz (310 g) FR cotton with a button front, adjustable cuffs and covered chest and sleeve pockets. The manufacturer states compliance with NFPA 2112.
Material and Construction
-
Material: 11 oz (310 g) FR cotton
-
Manufacturer-stated standard: NFPA 2112
- Stand collar, button closure and adjustable cuffs
- Covered chest pocket and sleeve pocket
-
Color: Black
Size Guide
| Size |
Neck |
Chest Width |
Sleeve |
Shoulder Width |
Length |
| M |
20.5" (52.1 cm) |
23.6" (59.9 cm) |
24.8" (63 cm) |
19.3" (49 cm) |
29.5" (74.9 cm) |
| L |
20.5" (52.1 cm) |
24.6" (62.5 cm) |
25.6" (65 cm) |
19.8" (50.3 cm) |
30" (76.2 cm) |
| XL |
20.9" (53.1 cm) |
25.6" (65 cm) |
26.4" (67.1 cm) |
20.4" (51.8 cm) |
30.5" (77.5 cm) |
| XXL |
20.9" (53.1 cm) |
26.6" (67.6 cm) |
27.2" (69.1 cm) |
20.9" (53.1 cm) |
30.9" (78.5 cm) |
| XXXL |
21.3" (54.1 cm) |
27.6" (70.1 cm) |
27.9" (70.9 cm) |
21.5" (54.6 cm) |
31.4" (79.8 cm) |
Manual measurements may vary by approximately 0.4" (1 cm). Use these garment measurements as a reference and allow room for underlayers.
Care and PPE Selection
Dry cleaning is recommended. If laundering is permitted by the sewn care label, do not exceed 165°F (74°C). Inspect the garment before use and select the complete PPE system according to the welding and workplace hazards.