E308LFC-O is a self-shielded stainless flux-cored wire for repair and light fabrication on compatible 304/304L, 308/308L, 321, and 347 stainless steels. It requires no external shielding gas and supports flat, horizontal, vertical, and overhead welding.
Materials and Applications
- 304 and 304L stainless steel
- 308 and 308L stainless steel
- 321 and 347 stainless steel
- Outdoor stainless repair, maintenance, and light fabrication
Key Specifications
-
Classification: E308LFC-O
-
Process: Flux-Cored
-
Shielding gas: Not required
-
Spool weight: 2 lb (0.9 kg)
-
Diameter options: .030" (0.8 mm) and .035" (0.9 mm)
-
Welding positions: Flat, horizontal, vertical, and overhead