Four configurations cover standard and aluminum wire for 24KD-style MIG guns. All configurations include gas nozzles, ceramic diffusers, M6 × 28 tip holders, and matching contact tips. Choose Standard .030", Standard .035", Aluminum, or Mixed Pack.
Works With
- 24KD-style MIG guns, including MB GRIP 24KD
- YESWELDER YWM-200
- YESWELDER YWM-211P
- YESWELDER DP200
Choose the Right Kit
.030" and .035" kits use standard contact tips for wire of the same diameter. Choose Aluminum for .035" and .045" aluminum wire, or Mixed Pack when both standard and aluminum contact tips are needed.
Included With Every Kit
- 2 × 12.5 mm Gas Nozzles, ICS0806
- 2 × Ceramic Gas Diffusers, ICF0539
- 5 × M6 × 28 Tip Holders, ICU0683
Kit Options
.030" (0.8 mm) option, 29 pieces:
- 20 × .030" (0.8 mm) Contact Tips, ICU0004-08
.035" (0.9 mm) option, 29 pieces:
- 20 × .035" (0.9 mm) Contact Tips, ICU0004-09
Aluminum option, 29 pieces:
- 10 × .035" (0.9 mm) Aluminum Contact Tips, ICU0004-59
- 10 × .045" (1.2 mm) Aluminum Contact Tips, ICU0004-62
Mixed Pack, 49 pieces:
- 10 × .030" (0.8 mm) Contact Tips
- 10 × .035" (0.9 mm) Contact Tips
- 10 × .035" (0.9 mm) Aluminum Contact Tips
- 10 × .045" (1.2 mm) Aluminum Contact Tips
Key Specifications
-
Gas nozzle diameter: 12.5 mm
-
Tip holder: M6 × 28
Front-End Requirements
Confirm that the MIG gun uses 24KD-style nozzles, ceramic diffusers, and M6 × 28 tip holders before ordering.