How To Weld Carbon Steel

How To Weld Carbon Steel

Table of Contents > 1. What Is Carbon Steel?
ย  ย ย 1.1 Types Of Carbon Steel
ย  ย ย 1.2 Why Is Welding Carbon Steel Challenging?
2. Welding Mild Steel (Low Carbon steel)
3. Welding Medium/High Carbon Steel
ย ย  ย ย 3.1 Filler Metal For High Carbon Steels
ย ย  ย ย 3.2 Heat Treatment
ย  ย  ย  ย  ย  ย 3.2.1 Post Heating Treatments
ย  ย  ย 3.3 Welding Methods For Carbon Steel Welding
4. Key Takeaways On Carbon Steel Welding
ย ๐ŸงHow To Weld Carbon Steel - FAQ
Steel is one of the most widely used materials in construction, manufacturing, and numerous other industries due to its strength, durability, and versatility. Steel is an alloy composed primarily of iron and varying amounts of carbon and other additives that give it desirable mechanical properties.

    Even though alloying elements make steel suitable for various applications, it can affect its weldability. Higher carbon content increases the hardness and toughness of steel, but it makes it more challenging to weld. That's why we'll explore how to weld carbon steel with different carbon content and explain what are the potential issues.

    TIG welding a gold cap on 5G carbon steel pipe
    TIG welding a gold cap on 5G carbon steel pipe.
    Photo by @weldtube (TikTok)

    What Is Carbon Steel?

    Carbon steel is an alloy composed primarily of iron and carbon. It's the most common type of steel and typically contains low amounts of other alloying elements. It is one of the most widely used materials in construction, manufacturing, and numerous other industries due to its strength, durability, and versatility.

    Keep in mind that all types of steel contain more than just iron and carbon. Modern steels only gain some of their strength from simple carbon additions but also from the added effect of small amounts of other alloying elements like manganese, silicon, chromium, molybdenum, vanadium, nickel, and copper. The amount of these elements is represented by the carbon equivalency formula, which will help you understand how the different alloying elements affect the hardness of the steel being welded.

    Elemental composition in weight percentage of various carbon steels used in this work

    ย 

    Elemental composition in weight percentage of various carbon steels used in this work.
    Source: https://www.researchgate.net/figure/Elemental-composition-in-weight-percentage-of-various-carbon-steels-used-in-this-work_tbl1_284179329

    Types Of Carbon Steel

    As the amount of carbon in the steel increases, the steel becomes harder, which is desirable when a piece is exposed to high wear and tear. As a result, we're seeing three different types of steel:

    • Low-carbon steel (less than 0.30% carbon)
    • Medium carbon steel (0.30%-0.60% carbon)
    • High carbon steel (0.60%-2% carbon)
    Carbon Steels composition

    Source: https://www.nuclear-power.com/nuclear-engineering/metals-what-are-metals/steels-properties-of-steels/

    Low-carbon steel is characterized by a low ratio of carbon to iron. It contains minimal amounts of carbon, typically less than 0.30%, and it is known as mild steel. The low amounts of carbon increase the ductility of the metal and make it cheaper to produce, which makes this type one of the most widely used. As a beginner or DIY and hobby welder, you are likely to deal with low-carbon steel or mild steel, and these are easiest to weld.

    low carbon steel
    Typical applications for low-carbon steel include automobile body components, structural shapes (e.g., I-beams, channel and angle iron), and sheets used in pipelines and buildings.
    Source: https://www.nuclear-power.com/nuclear-engineering/metals-what-are-metals/steels-properties-of-steels/low-carbon-steel/

    Medium carbon steel typically contains 0.30%-0.60% carbon, which balances the ductility and formability of low-carbon steel and the strength and hardness of high-carbon steel. With added chromium, nickel, and molybdenum, this type of steel is useful when creating items such as studs and gears that will encounter a lot of wear and tear. Due to higher carbon content, medium carbon steels are somewhat more challenging to weld.

    medium carbon steel gears
    Medium Carbon Steel Gears
    Source: https://www.reliance-foundry.com/blog/carbon-steel-mild-steel

    High carbon steel contains a carbon content ranging between 0.60% โ€“ 2%, which makes it highly corrosion-resistant, hard, and resistant to wear and tear. High carbon steels are often referred to as tool steel since it is widely used to make cutting tools, punches, dies, injection molding tools, ball and roller bearings for engines, and more. However, the higher carbon content also makes these steels more brittle and less ductile, causing cracking in the weld joint.

    high carbon steel

    Source: https://www.gardencityironandmetal.com/blog/whats-the-deal-with-high-carbon-steel/

    Why Is Welding Carbon Steel Challenging?

    When welding carbon steel, the heat from the welding process affects the surrounding material, creating what's known as the heat-affected zone (HAZ). Due to higher carbon equivalent, this zone can experience changes in microstructure when welded, leading to potential weaknesses or alterations in properties.

    heat affected zone HAZ

    Source: http://www.difference.minaprem.com/joining/difference-between-weld-metal-and-heat-affected-zone-haz/

    Firstly, high carbon content can lead to increased susceptibility to weld cracking. The carbon content in the metal can cause brittleness, leading to cracking during the cooling process. Rapid cooling during the welding process can result in martensite formation, a very hard but brittle microstructure in the weld area.

    The huge carbon content in the metal is also the leading cause of warping. Warping is the deformation of the metal during the cooling process, and it can happen because of the high carbon content in the metal. Traditionally, weld discoloration has emerged as an esthetic issue in carbon steel welding. However, it can also indicate other problems, such as a lack of fusion, porosity, and more.

    Warping in outer steel tube
    Warping in outer steel tube.
    Source: https://www.researchgate.net/figure/Warping-in-outer-steel-tube_fig10_292159144

    Therefore, welding carbon steel can be a daunting task, especially once the carbon content is high. However, there are certain precautions and procedures that can help you avoid cracking and other issues when welding carbon steel, so let's check them out.

    Welding Mild Steel (Low Carbon steel)

    As noted, low-carbon steels contain up to 0.30% carbon, which makes them highly ductile and easy to weld. As a result, you don't need heat treatment before or after the welding, and you can weld mild steel with one of the four most popular methods, such as Gas metal arc welding (MIG), TIG, Stick, or Flux Core.

    MIG welding mild steel is a common choice for beginners, as you need little to no prior experience to do it. You can choose matching filler metal according to the composition of the weld metal, and there is no pre or post-weld heat treatment required. Stick welding low-carbon steels is often preferred for quick on-field and outdoor repairs, and like with MIG, there are no specific precautions. You can use Flux core welding as a wire welding alternative for SMAW.

    mig welding mild steel
    MIG welding mild steel.
    Photo by @vxcxgaming (TikTok)

    TIG welding is often preferred when welding exotic or non-ferrous metals since it offers excellent heat control and provides high-quality welds. Still, you can use it to weld mild steel or any similar welding project with thinner material, but it requires more skill and experience.

    TIG welding mild steel
    TIG welding mild steel.
    Photo by @unimig (TikTok)

    Welding Medium/High Carbon Steel

    Things get tricky once the carbon is over 0.30% in the steel. The carbon reduces ductility and increases the strength so that the welds can become highly brittle and susceptible to cracking. As a result, welding high-carbon steel can be challenging and requires specific welding procedures. To successfully weld steel with medium to high carbon equivalency, you will need the right filler metal, heat input, and heat treatment.

    Filler Metal For High Carbon Steels

    Medium/high carbon steels are exceptionally hard, and their tensile strength can reach 35900 โ€“ 484000 psi. When welding such a high-strength steel material, there are two ways of thinking in selecting the welding consumables. You can either choose a filler that matches the strength of the base metal or consider a cracking issue and choose a lower-strength filler metal.

    However, of these two, it is more important to pay attention to the cracking risks of the welding joint. The harder the joint is, the bigger the chance that it will crack, so you will want to select the lower-strength filler metals when possible. As the joint has higher crack resistance, it is considered stronger, even if its overall strength is lower than two separate plates.

    Additionally, when selecting filler for steel with higher carbon quantities, you should avoid using electrodes with excessive hydrogen content. Diffusable hydrogen can cause cold cracking, so low-hydrogen electrodes are typically the best choice. These electrodes come with a designator of H2, H4, H8, or H16.

    AWS classification designators carbon steel diffusible hydrogen levels

    In specific cases, 309โˆ’type austenitic stainless steel welding consumables are recommended when welding high-carbon steels. Once again, the reason is low diffusable hydrogen content, which can cause cracking. The absence of hydrogen in this filler contributes to crack resistance together with the stable structure of the weld metal.

    309 austenitic stainless steel
    austenitic stainless steel
    Source: https://www.gpss.com/austenitic-stainless-steel/

    Heat Treatment

    Medium and high carbon steels require a specific pre and post-weld heat treatment to avoid cracking. Welding carbon steel in a room-temperature environment will cause rapid cooling, which leads to hardening and eventually cracking, so you will need pre- and post-heating processes. These processes are also known as the stress relief annealing process. This is the precise heat treatment in which carbon steel is heated to a particular temperature and cooled down slowly to make it ductile and malleable, increasing the overall weldability.

    Preheating the carbon steel before welding will promote slow cooling, remove moisture and hydrogen, and reduce the thermal stress into pieces. The preheat temperature will vary on the thickness and grade of the steel, and it is typically 300ยฐF to 500ยฐF. A high level of accuracy generally is not required for preheating carbon steels, but you don't want to go over 100ยฐF.

    Stress relief and post weld heat treatment
    Stress relief and post weld heat treatment.
    Source: https://www.metallurgyfordummies.com/what-is-stress-relieving.html

    Post Heating Treatments

    Post-heating processes are much more critical when welding medium and high-carbon steels. With the post-heat treatment right after welding, you will prolong the cooling rate, which increases the cracking resistance and decreases the hardness of HAZ. Carbon steel pieces can be post-heated through full annealing and soft annealing.

    Stress reduction as a function of annealing time for samples annealed in a nitrogen furnace at various temperatures
    Stress reduction as a function of annealing time for samples annealed in a nitrogen furnace at various temperatures.
    Source: https://www.researchgate.net/figure/Stress-reduction-as-a-function-of-annealing-time-for-samples-annealed-in-a-nitrogen_fig1_234871045
    • Full annealing includes slowly heating carbon steel to a holding temperature, which is 50 C (122 F) above the austenitic temperature (between 750-900 ยฐC / 1320-1652 ยฐF). After that, the pieces are cooled down slowly to the ambient temperature. The recommended cooling rate is 20 ยฐC (68 ยฐF) per hour. Once the parts reach 50 ยฐC (122 ยฐF), they can further be cooled to room temperature using air with natural draft.
    • Soft annealing is often used with high-carbon steels that require slower cooling rates. This process can last 12 to 48 hours. After welding, pieces are heated to the temperature of 800 ยฐC (1472 ยฐF). The metal is held at this temperature for 2-4 hours so that the structure fully converts into austenite. Next, the temperature is quickly brought down to 790 C (1454 ยฐF), and further cooling is controlled at a steady rate of 10 ยฐC (50 ยฐF) per hour until the temperature reaches 690 ยฐC (1274 ยฐF). The metal is then cooled to room temperature.
    • Welding carbon steel can also cause stress on the pieces, so that you can opt for stress-relief annealing. Welded components are heated up to the temperature of 600 to 650 C (1112 to 1202 F) and kept in this condition for an hour or more. Next, they are allowed to cool in the furnace till the temperature drops to 426 ยฐC (800 ยฐF), then cooled to ambient temperature slowly in the still air.ย 
    Soft Annealing And Stress Relieving
    Soft Annealing And Stress Relieving
    Source: https://link.springer.com/chapter/10.1007/978-3-658-39733-3_6

    Welding Methods For Carbon Steel Welding

    You can successfully weld carbon steel by using MIG welding, TIG welding, or Stick welding. Among these, MIG (Metal Inert Gas Welding) is a typical go-to choice since it is considered a low-hydrogen method that provides enough versatility. When MIG welding high carbon steels, make sure you reduce the heat and use a smaller wire diameter. High amperage can cause hot cracks in the weld joint, so avoid using too much heat.

    MIG welding Q235 carbon steel 3G
    MIG welding Q235 carbon steel 3G.
    Photo by @welding_yan (TikTok)

    Stick welding high-carbon steels is often preferred when welding thicker pieces. When using stick welding, make sure you opt for low-hydrogen electrodes. Hydrogen will cause cold cracking or delayed cracking, and even though post-heating will reduce the levels, try to avoid fillers with hydrogen.

    Welding E6010 on carbon steel 5P+
    Welding E6010 on carbon steel 5P+.
    Photo by @sewingwithfirewelding (TikTok)

    TIG welding carbon steel is often preferred on thinner pieces, where you want to avoid high heat that can cause brittleness and cracking. The key to successful welding is undermatching the filler metal, which means using a filler rod that is one or two grades lower than the base metal. When TIG welding fundamental projects, make sure you follow the American Welding Society welding procedure specifications.

    TIG welding Q235 carbon steel vertical welding
    TIG welding Q235 carbon steel vertical welding.
    Photo by @welding_yan (TikTok)

    Key Takeaways On Carbon Steel Welding

    • Welding low carbon steels (mild steel) is typically done at room temperature, without preheating or specific precautions.
    • As the carbon content increases, you will need to preheat and postheat the pieces to avoid cracking.
    • Preheating the carbon steel to 300-500 F before welding will promote slow cooling, remove moisture and hydrogen, and reduce the thermal stress into pieces.
    • Post-heating the pieces after the welding will prevent martensite formation, a very hard but brittle microstructure in the weld area.
    • Post-heating carbon steel can be done by full annealing, soft annealing, or stress-relief annealing. The key is to heat the pieces to create an austenite microstructure, which is malleable and ductile, and then let the parts cool slowly to avoid residual stresses and cracking.
    • Undermatch the filler metal. High-strength fillers will create strong welds that are prone to cracking.
    • Use low hydrogen rods. High hydrogen content will cause cold cracking or delayed cracking. After the use, you must store low hydrogen rods in the rod oven.
    • Avoid using too much heat. High amperages can cause thermal stress, causing cracks and other defects.

    ๐ŸงHow To Weld Carbon Steel- FAQ

    1. How to weld mild steel(low carbon steel)?

    MIG welding mild steel is a common choice for beginners, as you need little to no prior experience to do it. You can choose matching filler metal according to the composition of the weld metal, and there is no pre or post-weld heat treatment required. Stick welding low-carbon steels is often preferred for quick on-field and outdoor repairs, and like with MIG, there are no specific precautions. You can use Flux core welding as a wire welding alternative for SMAW.

    TIG welding is often preferred when welding exotic or non-ferrous metals since it offers excellent heat control and provides high-quality welds. Still, you can use it to weld mild steel or any similar welding project with thinner material, but it requires more skill and experience.

    2. What kind of filler metal for high carbon steels?

    When welding medium/high carbon steels with tensile strength ranging from 35,900 to 484,000 psi, the key consideration is minimizing cracking risks in the joint. While matching filler strength to the base metal is an option, prioritizing lower-strength filler metals enhances crack resistance, crucial for harder joints prone to cracking. For steels with higher carbon content, it's essential to avoid electrodes with excessive hydrogen to prevent cold cracking; opt for low-hydrogen electrodes labeled H2, H4, H8, or H16.

    ๐Ÿ‘ย You may be interested in the following:


    Leave a comment

    Please note, comments must be approved before they are published

    This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.