Welding 101
What Is MMA (Stick) Welding?

MMA welding, short for Manual Metal Arc welding, is commonly known as stick welding. In North America, the same process is formally called Shielded Metal Arc Welding (SMAW). It uses a flux-coated stick electrode to create an arc, add filler metal, and shield the weld pool from contamination.
Stick welding is popular because it works in situations where MIG or TIG can be harder to use. Since it does not need external shielding gas, welders often choose MMA for outdoor work, structural welding, farm repairs, and heavy equipment maintenance.
This guide covers the basics of MMA welding, including electrode choice, polarity, weldable metals, common applications, and how it compares with MIG and TIG welding.

Source: https://www.youtube.com/watch?v=rxXQ8UKSYK0&t
What Is MMA Welding?
MMA welding is a manual arc welding process that uses a consumable stick electrode. The rod does not feed automatically. The welder guides it by hand and replaces it when it becomes too short to use.
The machine provides the welding output, while the welder moves the electrode along the joint and feeds it forward as it burns down. Producing a consistent weld therefore takes practice and steady hand control.
MMA welding has been used for more than a century. Modern machines may include Hot Start, Arc Force, and Anti-Stick to help with arc starts, short arcs, and stuck electrodes. These features assist the welder, but they do not automate the process.
How Does Stick Welding Work?
The electrode holder and work clamp connect to the stick welder through welding leads. When the rod touches the workpiece, it completes the electrical circuit. Tapping or scratching the rod against the metal and then lifting it slightly starts the arc.
The heat from the arc melts the end of the rod and the surface of the base metal, creating a weld pool. As welding continues, the metal core of the electrode melts into the pool as filler metal.
At the same time, the heat breaks down the flux coating. This creates shielding gases that keep air away from the molten metal. It also forms slag, which covers the bead while it cools.
After the weld cools, the slag is chipped away and the surface is cleaned with a wire brush. The bead can then be inspected. On a multipass weld, all slag must be removed before the next pass so it does not become trapped between layers.

Source: https://www.corrosionpedia.com/stick-welding-a-comprehensive-guide-to-a-very-popular-welding-process/2/6885
Common Stick Welding Electrodes and Polarity
E6010, E6011, E6013, and E7018 are the stick electrodes most commonly used on carbon steel. The right rod depends on the job, the base metal, and the type of current the welder provides.
On a DC welder, DCEP means the electrode holder connects to the positive terminal. DCEN means it connects to the negative terminal.
| Electrode | Best Used For | Typical Polarity |
|---|---|---|
| E6010 | Deep penetration, root passes, and pipe welding | DCEP |
| E6011 | Repair work and lightly rusted steel | AC or DCEP |
| E6013 | Light fabrication, practice, and a smooth arc | AC, DCEN, or DCEP |
| E7018 | Structural welding and low-hydrogen work | DCEP or AC, depending on the rod |
The electrode classification provides information about strength, welding position, coating type, and usable current. E7018 and other low-hydrogen electrodes must also be kept dry.
Always check the rod package for the recommended amperage and polarity because requirements can vary by manufacturer. Our guide to choosing the right stick electrode explains rod classifications and selection in more detail.
Stick Welding Positions
Stick welding can be used in different positions, depending on the electrode and the joint.
The main stick welding positions are:
- Flat (1F): Usually the easiest position and a good place to practice.
- Horizontal (2F): Common in fabrication and structural work.
- Vertical (3F): Used when the joint cannot be moved into a flat position.
- Overhead (4F): Usually the most difficult position and requires careful control of the weld pool.
Not every electrode is suitable for every position. Check the rod classification to confirm whether it is intended for flat, horizontal, or all-position welding.
Overhead welding takes more control because hot slag and molten metal can fall toward the welder.

Source: https://www.youtube.com/watch?v=DW9IE6jYDmc
What Metals Can You Weld With Stick Welding?
Stick welding is mainly used on carbon steel, especially mild steel. With the correct electrode, it can also weld stainless steel and cast iron. It is possible to weld aluminum and copper with stick welding, but neither is a common choice for the process.
| Metal | Stick Welding Suitability |
|---|---|
| Carbon steel | The most common and practical choice |
| Stainless steel | Use an electrode matched to the stainless grade |
| Cast iron | Mainly used for repairs with nickel-based rods and careful heat control |
| Aluminum | Possible with aluminum electrodes, but difficult to control |
| Copper | Rarely used; TIG or MIG is usually preferred |
The electrode type must match the base metal. Rod diameter and amperage should suit the material thickness and joint. Polarity should follow the instructions on the rod package.
Common Applications of Stick Welding
Stick welding is often used when steel needs to be repaired or welded in place.
Common applications include:
- Farm and ranch repairs
- Trailer and heavy equipment repair
- Structural steel and jobsite welding
- Pipeline and root pass welding
- Plant maintenance and repair
- Garage and home shop projects
Many of these jobs involve large or fixed parts that are difficult to move. Stick welding lets the welder bring the equipment to the work instead of moving the workpiece back to a shop.

Source: https://www.youtube.com/watch?v=Nzaar389BE4
Pros and Cons of Stick Welding
Stick welding is useful, but it is not the best process for every job.
🟢 Pros
- Works outdoors without a shielding gas cylinder
- Uses a simple, portable setup
- Can weld in all positions with the right electrode
- Works well on medium to thick steel
- Handles light surface rust better than MIG or TIG
🔴 Cons
- Takes more practice to learn than MIG welding
- Produces more spatter than TIG welding
- Requires slag removal on multipass welds
- Can be difficult to control on thin sheet metal
- Requires rod changes during longer welds
MMA vs MIG vs TIG Welding
MMA, MIG, and TIG all use an electric arc, but they differ in how filler metal is added and how the weld pool is protected.
| Process | Electrode and Filler Metal | Shielding |
|---|---|---|
| MMA / Stick | Consumable flux-coated stick electrode | Shielding comes from the flux coating |
| MIG | Continuously fed consumable wire | External shielding gas |
| TIG | Non-consumable tungsten electrode; filler is added separately when needed | External shielding gas |
Start with the workpiece and location when choosing a process. MMA is a good fit when a steel part must be repaired in place or the equipment needs to move with the job. If you are still deciding which process fits your work, compare MIG, TIG, Stick, and Flux-Core welding side by side.
Who Should Choose MMA Welding?
Choose stick welding if you need a portable welding process for steel repair, maintenance, or outdoor work. It is also a good choice when wind makes gas-shielded processes less practical.
MMA is less suitable for thin sheet metal, long production welds, or projects where appearance is the main concern. Electrode changes and slag removal can slow down this type of work.
If these advantages and limitations fit your projects, MMA is a practical welding process worth learning.
Source: https://www.youtube.com/watch?v=QPXjpo_AFuY&t
Beginner Tips for Better Stick Welds
Keep your first practice sessions simple. Wear the proper PPE and practice on clean scrap steel. Start in the flat position.
Follow these beginner tips:
-
Choose a rod type and size that match the metal and joint.
-
Start within the amperage range printed on the rod package.
-
Keep the arc short and steady.
-
Maintain a steady rod angle and travel speed.
-
Remove all slag before adding another pass.
-
Store E7018 and other low-hydrogen rods in a dry place.
Once your beads become more consistent, try harder joints and welding positions. Practice one skill at a time so you can see what each adjustment changes.

Source: https://www.youtube.com/watch?v=HKfAd6CJZ8Y&t
Conclusion
MMA welding looks simple because the equipment is basic, but the welder still controls what happens at the arc. The machine can help with arc starts and reduce electrode sticking, but it cannot maintain the correct rod angle, arc length, or travel speed for you.
Once you can control those fundamentals consistently, MMA becomes a practical process for steel repairs, structural work, and outdoor welding.
Frequently Asked Questions
1. Are MMA, SMAW, and stick welding the same?
Yes. MMA, SMAW, and stick welding refer to the same manual arc welding process. The preferred term varies by region, but each name describes welding with a manually controlled, flux-coated stick electrode.
2. Does MMA welding need shielding gas?
No. MMA welding does not need an external shielding gas cylinder. The electrode coating produces shielding gases and slag as it breaks down during welding.
3. Is stick welding good for beginners?
Beginners can learn stick welding, but it usually takes more practice than MIG welding. Starting the arc and maintaining the correct arc length are often the first challenges.
4. What is stick welding best used for?
Stick welding is commonly used for steel repair, structural work, equipment maintenance, pipeline welding, and jobs where the workpiece cannot easily be moved.
5. What are the most common stick welding rods?
E6010, E6011, E6013, and E7018 are common rods for carbon steel. There is no single best electrode because the correct choice depends on the machine, metal condition, welding position, and required weld properties.
6. What is the difference between stick welding and MIG welding?
Stick welding uses a flux-coated electrode that creates its own shielding, while MIG welding uses a continuous wire electrode and external shielding gas. Stick welding is often preferred for outdoor work and repairs, while MIG welding is usually easier to learn and better suited for clean indoor projects.