E7018 10LB Welding Rod Low Hydrogen Carbon Steel Stick Electrodes
E7018-10LB-2.4
- Free Contiguous US Shipping Over $150
- In stock, ready to ship
- Inventory on the way
The E7018 is a low-hydrogen, iron powder electrode known for producing high-quality, X-ray-grade welds. It can be used in all positions with either AC or DC reverse polarity welding currents.
Features:
- Suitable for all-position welding, this electrode is ideal for welding medium-grade carbon steels without preheating, as well as cold-rolled steels that typically exhibit excessive porosity with conventional electrodes.
- Offers a steady arc, low spatter, excellent re-striking ability, and high deposition efficiency.
Applications:
Perfect for use on low-alloy structural components, low to high carbon steels, offshore rigs, power plants, steel structures, and for tack welding in tubular wire applications.
Specifications:
- Diameter: 3/32'', 1/8", 5/32"
- Length: 14''
- Weight: 10 lbs
- Recommended Amperage: 70-100A, 115-165A,150-220A