Quick Look
- DC TIG pulse
- Key Feature
- LED
- Display
- Steel / Stainless
- Material Compatibility
- ≤ 1/2" (13 mm) @ 220V
- Recommended Thickness
- 200A
- Max Output
- TIG / Stick
- Processes
- 110V / 220V
- Input Voltage
- AC/DC TIG for aluminum
- Key Feature
- LED
- Display
- Steel / Stainless / Aluminum
- Material Compatibility
- ≤ 1/4" (6.4 mm) @ 220V
- Recommended Thickness
- 200A
- Max Output
- TIG / Stick
- Processes
- 110V / 220V
- Input Voltage
- Built-in pump + CNC
- Key Feature
- LED
- Display
- Steel / Stainless / Aluminum
- Material Compatibility
- ≤ 1/4" (6 mm) @ 220V
- Recommended Thickness
- 200A
- Max Output
- TIG / Stick / Plasma
- Processes
- 96-265V
- Input Voltage
Power & Output
Input Voltage
110V, 220V ±15% 50/60Hz
110V, 220V ±15% 50/60Hz
Single-phase 96-265V 50/60Hz
Processes
DC TIG (Pulse), Stick
AC/DC/MIX TIG (Pulse), Stick
AC/DC TIG (Pulse), Stick, Plasma (Built-in Pump)
Output Current Range
TIG: 10-160A @ 110V; 10-200A @ 220V Stick: 20-140A @ 110V; 20-160A @ 220V
TIG: 10-140A @ 110V; 10-200A @ 220V Stick: 20-120A @ 110V; 20-160A @ 220V
TIG: 5-160A @ 110V; 5-200A @ 220V Stick: 10-160A @ 110V; 10-200A @ 220V Plasma: 12-25A @ 110V; 12-45A @ 220V
Material & Capability
Material Compatibility
TIG: Steel, Stainless Steel Stick: Steel
TIG: Steel, Stainless Steel, Aluminum Stick: Steel
TIG: Steel, Stainless Steel, Aluminum Stick: Steel Plasma: Steel, Stainless Steel, Aluminum
Recommended Thickness
TIG: ≤ 3/16" (5 mm) @ 110V; ≤ 1/2" (13 mm) @ 220V Stick: ≤ 1/4" (6 mm) @ 110V; ≤ 1/2" (13 mm) @ 220V
TIG: ≤ 3/16" (4.8 mm) @ 110V; ≤ 1/4" (6.4 mm) @ 220V Stick: ≤ 3/16" (4.8 mm) @ 110V; ≤ 1/4" (6.4 mm) @ 220V
TIG: ≤ 5/32" (4 mm) @ 110V; ≤ 3/16" (5 mm) @ 220V Stick: ≤ 3/16" (5 mm) @ 110V; ≤ 1/4" (6 mm) @ 220V
Clean Cut Thickness
Not applicable
Not applicable
3/8" (10 mm) @ 110V 19/32" (15 mm) @ 220V
Severance Cut Thickness
Not applicable
Not applicable
3/4" (20 mm) @ 110V 1 3/16" (30 mm) @ 220V
TIG
TIG Ignition Type
HF Start
HF Start
HF Start
Foot Pedal Compatibility
Supported
Supported
Supported
Tungsten Type
WT20, WC20, WL20, WL15
WT20, WC20, WL20, WL15, WP
WT20, WC20, WL20, WL15, WP
Tungsten Diameter
≤ 5/32" (4.0 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V
≤ 1/8" (3.2 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V
≤ 5/32" (4.0 mm)
TIG Torch Type
WP-17 (M16 × 1.5 connector, 5-pin control cable)
WP-26 (M16 × 1.5 connector, 5-pin control cable)
WP-26 (M16 × 1.5 gas connector, KDP35-50 electric connector, 5-pin control cable)
TIG Filler Rod Material
ER70S-6, ER308L
ER70S-6, ER308L, ER4043
ER70S-6, ER308L, ER4043
TIG Filler Rod Diameter
≤ 1/8" (3.2 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V
≤ 1/8" (3.2 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V
≤ 3/32" (2.4 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V
Gas Requirements
100% Argon
100% Argon
100% Argon
Consumables Compatibility
WP-17 / WP-18 / WP-26
WP-17 / WP-18 / WP-26
WP-17 / WP-18 / WP-26
Stick
Stick Electrode Type
E6011 / E6013 / E7018
E6010 / E6011 / E6013 / E7018
E6010 / E6011 / E6013 / E7018
Stick Electrode Diameter
≤ 3/32" (2.4 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V
≤ 5/32" (4.0 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V
≤ 3/32" (2.4 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V
Plasma Cutting
Pilot Arc
Not applicable
Not applicable
Supported
Plasma Arc Starting
Not applicable
Not applicable
Back-flow Start
Air Pressure
Not applicable
Not applicable
45-60 PSI @ 110V; 55-75 PSI @ 220V
Air Flow
Not applicable
Not applicable
≥ 6.0 CFM
Recommended Compressor
Not applicable
Not applicable
30-60 gal, ≥ 2 HP
Plasma Torch Type
Not applicable
Not applicable
IPL50 (M16 × 1.5 connector, 5-pin control cable)
CNC Capability
Not supported
Not supported
CNC ready
Gas Requirements
Not applicable
Not applicable
Compressed Air
Consumables Compatibility
Not applicable
Not applicable
IPL50-45
Physical & Safety
Display
LED
LED
LED
Fan Control
Continuous Fan Mode
Fan on Demand
Fan on Demand
App Control
Not supported
Not supported
Not supported
Weight
10.7 lbs
19.59 lbs
44.9 lbs
Dimensions
13.98" × 6.1" × 9.45"
15.7" × 7.09" × 9.84"
18.5" × 13.6" × 8.7"
Protection Features
Overheat Overcurrent Overvoltage
Overheat
Overheat Overcurrent VRD (Voltage Reduction Device) - Stick
General
Input Current
50A @ 110V; 40A @ 220V
50A @ 110V; 40A @ 220V
50A @ 110V; 40A @ 220V
Open Circuit Voltage (OCV)
TIG/Stick: 65V
TIG/Stick: 75V
TIG: 68V Stick: 68V (VRD: 7V) Plasma: 312V
Generator Compatibility
Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.
Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.
Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.
Cable Length
Ground: 10 ft (3 m) TIG Torch: 13 ft (4 m)
Ground: 10 ft (3 m) TIG Torch: 13 ft (4 m)
Ground: 10 ft (3 m) TIG Torch: 13 ft (4 m) Plasma Torch: 13 ft (4 m)
Power Cord Length
6.5 ft (2 m)
6.5 ft (2 m)
6.5 ft (2 m)
Certification
CE, ETL, UL
CE, ETL, UL
Not applicable
Warranty
2 Years
2 Years
3 Year