YesWelder

Compare All Welders

Gasless Starter Kit Hardware > Tools > Welders & Plasma Cutters YesWelder

FLUX-135PRO

Gasless flux-core 3-in-1 that runs on any 110V outlet.

From $159.00

or 4 payments of $39.75 with Klarna*

Learn more
YWM-160 Flexible Manual MIG Controlled Multi-process MIG Welder

YWM-160

Compact manual-control MIG for everyday steel work.

From $226.00

or 4 payments of $56.50 with Klarna*

Learn more
ARC-125DS-PRO 110V Mini Portable Stick Welder Hardware > Tools > Welders & Plasma Cutters YesWelder Welder

ARC-125DS-PRO

A stick welder that fits in one hand — 4.4 lbs, 110V.

From $79.00

or 4 payments of $19.75 with Klarna*

Learn more

Quick Look

Synergic flux-cored
Key Feature
LED
Display
Steel / Stainless
Material Compatibility
≤ 3/16" (5 mm) @ 110V
Recommended Thickness
135A
Max Output
Flux / TIG / Stick
Processes
110V
Input Voltage
160A synergic MIG
Key Feature
LED
Display
Steel / Stainless
Material Compatibility
≤ 5/16" (8 mm) @ 220V
Recommended Thickness
160A
Max Output
MIG / Flux / TIG / Stick
Processes
110V / 220V
Input Voltage
Compact Stick/TIG
Key Feature
LED
Display
Steel
Material Compatibility
≤ 1/4" (6 mm) @ 110V
Recommended Thickness
125A
Max Output
Stick / TIG
Processes
110V
Input Voltage

Power & Output

Input Voltage

110V ±10% 50/60Hz

110V, 220V ±10% 50/60Hz

110V ±10% 50/60Hz

Processes

Flux-Cored, Lift TIG, Stick

MIG, Flux-Cored, Lift TIG, Stick

Stick, Lift TIG

Output Current Range

Flux-Cored: 35-135A @ 110V TIG: 15-135A @ 110V Stick: 20-135A @ 110V

MIG: 40-120A @ 110V; 40-160A @ 220V TIG: 20-120A @ 110V; 20-160A @ 220V Stick: 20-120A @ 110V; 20-160A @ 220V

Stick: 20-125A

Duty Cycle

Flux-Cored: 60% @ 135A1

MIG: 60% @ 160A1

Stick: 60% @ 125A1

Material & Capability

Material Compatibility

Flux-Cored: Steel, Stainless Steel TIG: Steel, Stainless Steel Stick: Steel

MIG: Steel, Stainless Steel TIG: Steel, Stainless Steel Stick: Steel

Stick: Steel TIG: Steel

Recommended Thickness

Flux-Cored: ≤ 3/16" (5 mm) @ 110V TIG: ≤ 5/32" (4 mm) @ 110V Stick: ≤ 3/16" (5 mm) @ 110V

MIG: ≤ 3/16" (5 mm) @ 110V; ≤ 5/16" (8 mm) @ 220V TIG: ≤ 5/32" (4 mm) @ 110V; ≤ 1/4" (6 mm) @ 220V Stick: ≤ 3/16" (5 mm) @ 110V; ≤ 5/16" (8 mm) @ 220V

Stick: ≤ 1/4" (6 mm) @ 110V TIG: ≤ 5/32" (4 mm) @ 110V

MIG

Synergic Function

Supported

Supported

Not applicable

Spool Gun Compatibility

Not supported

Not supported

Not applicable

MIG Wire Type

E71T

ER70S-6 / E71T / ER308L

Not applicable

Wire Diameter

.030" (0.8 mm) / .035" (0.9 mm)

.023" (0.6 mm) / .030" (0.8 mm) / .035" (0.9 mm)

Not applicable

MIG Torch Type

YW-FLUX135 (10-25 connector, 2-pin control cable)

Built-in

Not applicable

Gas Requirements

No gas (Flux-Cored)

CO2 100%, Mix Gas, Argon 100%

Not applicable

Wire Feed Mechanism

2-Roll

2-Roll, 4-Roll

Not applicable

Consumables Compatibility

Magnum 100L

Magnum 100L

Not applicable

TIG

TIG Ignition Type

Lift Start

Lift Start

Lift Start

Foot Pedal Compatibility

Not supported

Not supported

Not supported

Tungsten Type

WT20, WC20, WL20, WL15

WT20, WC20, WL20, WL15

WT20, WC20, WL20, WL15

Tungsten Diameter

≤ 3/32" (2.4 mm) @ 110V

≤ 3/32" (2.4 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V

≤ 3/32" (2.4 mm) @ 110V

TIG Torch Type

WP-17V-10 (Optional. Sold separately.)

WP-17V-10 (Optional. Sold separately.)

WP-17V-10 (Optional. Sold separately.)

TIG Filler Rod Material

ER70S-6, ER308L

ER70S-6, ER308L

ER70S-6, ER308L

TIG Filler Rod Diameter

≤ 3/32" (2.4 mm) @ 110V

≤ 3/32" (2.4 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V

≤ 3/32" (2.4 mm) @ 110V

Gas Requirements

100% Argon

100% Argon

100% Argon

Consumables Compatibility

WP-17 / WP-18 / WP-26

WP-17 / WP-18 / WP-26

WP-17 / WP-18 / WP-26

Stick

Stick Electrode Type

E6011 / E6013 / E7018

E6011 / E6013 / E7018

E6011 / E6013 / E7018

Stick Electrode Diameter

≤ 1/8" (3.2 mm) @ 110V

≤ 1/8" (3.2 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V

≤ 1/8" (3.2 mm) @ 110V

Plasma Cutting

CNC Capability

Not supported

Not supported

Not supported

Physical & Safety

Display

LED

LED

LED

Fan Control

Continuous Fan Mode

Continuous Fan Mode

Continuous Fan Mode

App Control

Not supported

Not supported

Not supported

Weight

10.98 lbs

20.51 lbs

4.4 lbs

Dimensions

14.57" × 6.1" × 8.66"

17.52" × 6.5" × 11.61"

9.3" × 3.7" × 5.1"

Protection Features

Overheat Overcurrent

Overheat Overcurrent

Overheat Overcurrent Undervoltage

General

Input Current

50A

50A @ 110V; 40A @ 220V

50A

Open Circuit Voltage (OCV)

Flux-Cored/TIG/Stick: 65V

MIG/TIG/Stick: 60V

Stick/TIG: 60V

Generator Compatibility

Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.

Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.

Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.

Cable Length

Ground: 6.5 ft (2 m) MIG Gun: 8 ft (2.5 m)

Ground: 10 ft (3 m) MIG Gun: 10.5 ft (3.2 m)

Ground: 6.5 ft (2 m)

Power Cord Length

5.9 ft (1.8 m)

6.5 ft (2 m)

6 ft (1.85 m)

Certification

CE, ETL, UL

UL

CE, ETL, UL

Warranty

2 Years

3 Year

2 Years

1. Detailed Duty Cycle

FLUX-135PRO: Flux-Cored: 60% @ 135A; 100% @ 104A · TIG: 60% @ 135A; 100% @ 104A · Stick: 60% @ 135A; 100% @ 104A

YWM-160: MIG (110V): 60% @ 120A; 100% @ 93A · MIG (220V): 60% @ 160A; 100% @ 126A · TIG (110V): 60% @ 120A; 100% @ 93A · TIG (220V): 60% @ 160A; 100% @ 126A · Stick (110V): 60% @ 120A; 100% @ 93A · Stick (220V): 60% @ 160A; 100% @ 126A

ARC-125DS-PRO: Stick: 60% @ 125A; 100% @ 97A

*Financing available to qualified customers through Klarna. Pay-in-4 and monthly options are subject to eligibility and approval; see checkout for available plans and terms. Prices shown are starting prices for each model and may vary by configuration.