CUT-55DS
Pilot Arc Non-Touch Plasma Cutter / Dual Voltage 110/220V / IGBT Inverter Portable Cutting Machine
FEATURES
- Non-Touch Pilot Arc.
- Dual Voltage 110/220V.
- Powerful 1/2" Clean Cut.
- IGBT Inverter Technology.


Portability
IGBT inverter, smaller size and lighter weight, and higher reliability allows you to take to wherever the job is needed.

Built-in Post Flow
When you stop cutting, the air runs on for a minute to cool the consumable of the plasma cutter torch. This will extend consumable life.

DUAL VOLTAGE
Capable to run directly on 110 V (±10%) 50/60 Hz power or on 220 V (±10%) 50/60 Hz with the use of a power adapter.

55Amp Non-Touch Pilot Arc Plasma Cutter cuts up to 3/4". Designed for both demanding industrial and construction work, or home and hobby use.
Cutting Material: Stainless steel, Alloy steel, Mild steel, Copper, Cast Iron and Chrome.
The pilot arc torch efficiently cuts through rough, painted, and rusty surfaces, while producing minimal slag.
Pilot arc technology allows you to cut without touching the tip of the metal, for better quality and longer consumable life.


Max Rated Clean Cut Thickness: 5/16"@110V, 1/2"@220V.
Max Severance Thickness: 15/32"@110V, 3/4"@220V.
1. Power Indicator
2. Overheat Indicator
3. Torch Protection Indicator
4. Air Pressure Gauge
5. 2/4T Function
6. Gas Checking
7. Cutting
8. Current Display
9. Amperage Setting


PRODUCT WEIGHT: 14.55lb
PRODUCT DIMENSIONS: 16.14 "* 6.49" * 11.81"
INPUT VOLTAGE: 110V/220V 50/60 Hz
INPUT CURRENT: recommend 63A breaker
CUTTING RECOMMENDATION:
Output Current 20A @110V @50.8PSI
Output Current 40A @220V @58-65PSI
DUTY CYCLE: 100%@35A, 60%@55A
POST FLOW TIME BUILT-IN: 20s
AIR COMPRESSOR REQUIREMENT: 5-7CFM @60PSI
WELDING MATERIAL: stainless steel, alloy steel, mild steel, copper, and aluminum, and other color metal materials
PROTECTION CLASS: IP21S