ER4043/1LB-0.9 MIG Welding Wire
Silicon Aluminum MIG Welding Wire
 1LB Spool .035" Silicon Aluminum MIG Welding Wire
ER4043/1LB-0.9 1LB Spool .035" Silicon Aluminum MIG Welding Wire
3 pieces 1LB Spool .035" Silicon Aluminum MIG Welding Wire
5 pieces 1LB Spool .035" Silicon Aluminum MIG Welding Wire

ER4043/1LB-0.9 1LB Spool .035" Silicon Aluminum MIG Welding Wire

ER4043/1LB-0.9

Regular price23.00
/
Quantity
  • Free Contiguous US Shipping Over $150
  • In stock, ready to ship
  • Inventory on the way

Aluminum welding wire ER4043 is a general-purpose type aluminum welding wire. It contains silicon additives, which result in improved fluidity (wetting action) of the weld pool and also produces a weld less sensitive to cracking. Its bright weld finish makes it a popular choice of welders. It can be used to weld various grades of aluminum.

  • 5% silicon aluminum (AlSi5) filler metal welding wire for MIG welding process.
  • The silicon additions result in improved fluidity (wetting action) to make the alloy a preferred choice by welders. Less sensitive to weld cracking and produces brighter.
  • It can be used to weld various grades of aluminum, 3003, 3004, 5052, 6061, 6063, and casting alloys 43, 355, 356, and 214.

Most items are usually shipped within 3-5 working days. Your delivery confirmation email will contain your tracking number and order details. Should you have any questions, our team is also on hand 7 days a week and can be reached at support@yeswelder.com.

This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.