YesWelder

Common TIG Welding Defects And How To Deal With Them

TIG welding, or Gas Tungsten Arc Welding, is complex but delivers high-quality, visually appealing welds, especially on stainless steel and non-ferrous metals like aluminum. Beginners need time and patience to master it and will face various challenges. That’s why we decided to explain the common TIG welding defects and share a few tips on how to solve them.

Continue reading
TIG Root Pass Techniques Explained

Welding materials over 1/2” thick requires a beveled joint and a root pass to establish a strong foundation. In this article, we'll explain TIG root pass techniques and challenges and present tips for successful operation.

Continue reading
Right TIG Filler Rods For Different Metals
Choosing the right TIG filler rods for different metals is crucial for creating strong welds, but the vast selection can be overwhelming. The American Welding Society has classified TIG filler rods to simplify the selection process, and in this guide we’ll explain everything closely.
Continue reading