YesWelder® 150AMP Spool Gun | Aluminum Welding Gun Torch - YesWelder
YesWelder® 150AMP Spool Gun | Aluminum Welding Gun Torch - YesWelder
YesWelder® 150AMP Spool Gun | Aluminum Welding Gun Torch - YesWelder

LBT150 150AMP Aluminum Welding Spool Gun

LBT150

Regular price189.99
/

  • Free Contiguous US Shipping Over $150
  • In stock, ready to ship
  • Inventory on the way

The torch could be connected with the welding machine or the control device, equipped with different diameter welding wires and conductive tips, and passes through the protective cooling gas Ar 99.99%, which can be used for aluminum 99.99% argon gas welding
Recommended for use with YesWelder MIG-270K, YWM-200, YWM-211P, MIG-205DS-B, MIG-250PRO-SG welder.

Description

Spool Gun: LBT150
Duty Cycle: 60%
Cooling: Air-cooled
Connector: European connector
Motor voltage: DC 24V
Wire Spool: D100/ 4’’
Aluminum Wire Size: .030"-.045”
U Knurl groove: .30”/.035”. 039”/.045"

Suitable for softer wire

The LBT150 Spool Gun features a 10’ direct connect cable, perfect for MIG welding softer wires, such as aluminum. The torch itself has a built-in wire spool and wire feeder, which reduces the distance that the wire needs to travel.  

Visibility for the moving wire

Clear plastic housing allows for full visibility of all moving parts, allowing you to ensure that your wire is feeding smoothly and consistently. You also have a clear view of your wire spool, so that you know when you need to replace it.

Most items are usually shipped within 3-5 working days. Your delivery confirmation email will contain your tracking number and order details. Should you have any questions, our team is also on hand 7 days a week and can be reached at support@yeswelder.com.

This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.

Customer Reviews

Based on 28 reviews
71%
(20)
14%
(4)
7%
(2)
0%
(0)
7%
(2)
A
Andre St-Germain
Excellent support

Hello.
I received the "LBT150 150AMP Aluminum Welding Spool Gun" broken during shipping, and I couldn't use it. I contacted Yeswelder support, and Raymond sent me a new "LBT150 150AMP Aluminum Welding Spool Gun."
Thanks to Raymond for his excellent support.

R
Ronald Harrison
Spool gun

Works great light wait

c
cameron h mooney
Easy welding in ten minutes

Third gun was a charm..one broken ,one faulty...but this one welds sweetly. First welds were a little hot but with one adjustment had it looking close to tig with full penetration
Welds as well as my Miller, which was ten times the price. For quick setup small jobs this will be my go to welder. Perfect for anyone getting who wants an excellent budget welder.

A
Anonymous
Spool gun purchase for 205ds

Advertisement needs to be more specific about what model the spool gun works with. I purchased the spool gun being led to believe it would work with my welder but in fact it won't. Only works with newer model 205 ds

J
Jarrette Byington
Inconsistent feeding/defective

Failed to feed on first use. I purchased this and didn’t have a project to use it on right away but when I did finally get to use it, the drive roller would spin but wouldn’t feed wire. I couldn’t even get it to feed correctly with the contact tip removed, drive roller fully tensioned and spool fully loose. I contacted them about it and they confirmed it was a defective unit but that it was out of warranty. They offered me a 15% off coupon code but that is offered to any new customer and they “run specials” with more of a discount. Why would I buy another unit after this terrible customer support experience.. I would suggest to stay away from this company because other companies like everlast or esab would make this right the first time even out of warranty.