Video Review
YesWelder CUT-65DS PLUS Review: 4-in-1 Plasma Cutting Tests by BULLI KID

Quick Verdict
The YesWelder CUT-65DS PLUS is a 4-in-1 plasma cutter designed for metal cutting, grid cutting, gouging, and marking applications.
In this review, BULLI KID unboxes and tests the CUT-65DS PLUS through hands-on cutting projects, including mild steel cutting, aluminum cutting, grid cutting, plasma gouging, and plasma marking.
The video focuses on the overall user experience of the machine, including setup, torch design, digital controls, cut quality, arc stability, and how each cutting mode performs in practical use.
During testing, BULLI KID highlights the machine's simple setup, smooth arc performance, compact design, and the convenience of switching between different plasma functions in one unit.
For welders, fabricators, and hobbyists looking for a versatile plasma cutter for garage projects, repair work, and general metal fabrication, this review provides a practical look at how the CUT-65DS PLUS performs beyond its specifications.
About the YesWelder CUT-65DS PLUS
The YesWelder CUT-65DS PLUS is a dual-voltage plasma cutter designed for metal fabrication, repair work, and general cutting applications.
Unlike a basic plasma cutter focused only on cutting, the CUT-65DS PLUS combines four plasma functions in one machine:
- Plasma cutting
- Grid cutting
- Plasma gouging
- Plasma marking
Key capabilities include:
- 4-in-1 Plasma Functions: Supports plate cutting, grid cutting, gouging, and marking for different fabrication applications.
- Dual Voltage Operation: Supports both 110V and 220V input for different working environments.
- Digital Control System: Provides adjustment options for cutting current, air pressure settings, post-flow timing, and cutting modes.
- Built-In Air Management: Includes an integrated air separator to help manage compressed air supply.
- 2T / 4T Operation: Provides different trigger control options depending on cutting preference.
The CUT-65DS PLUS is designed for users who need a plasma cutter for standard cutting tasks. It also adds extra functions for fabrication and preparation work, including grid cutting, gouging, and marking.
Recommended Products
Recommended Products
Reviewer Information
| Field | Details |
|---|---|
| Reviewer | BULLI KID |
| YouTube Channel | @BulliKid |
| Channel Focus | Welding, fabrication, tools, and hands-on equipment testing |
| Review Focus | Plasma cutting, grid cutting, gouging, marking, and machine setup |
| Product Tested | YesWelder CUT-65DS PLUS |
CUT-65DS PLUS Testing Overview
| Test Item | Details |
|---|---|
| Product Tested | YesWelder CUT-65DS PLUS |
| Power Source Tested | 120V garage power (220V capability discussed) |
| Materials Tested | Mild steel tubing, steel sections, thin-wall aluminum, grid material |
| Functions Tested | Plate cutting, grid cutting, gouging, marking |
| Main Focus | Setup, cut quality, arc stability, and ease of operation |
Full Review: BULLI KID Tests the YesWelder CUT-65DS PLUS
Compact Design and Setup
One of the first things shown in the review is the compact size of the CUT-65DS PLUS.
BULLI KID notes that the machine is lightweight enough to hold with one hand, making it easy to move around compared with larger plasma cutters.
The setup process is straightforward:
- Connect the ground cable
- Connect the plasma torch
- Connect the air supply
Compared with older designs that required multiple cable connections, the CUT-65DS PLUS features a cleaner connection layout.
The review also highlights the torch design. BULLI KID points out the comfortable grip, rubberized section for better handling, and swivel design that helps reduce cable tension during operation.
The machine was tested using a standard garage power setup at 120V, while the reviewer also notes that 220V operation is available for users who need additional cutting capability.
Plasma Cutting Performance
The first cutting tests focused on standard plasma cutting.
BULLI KID starts with settings around 55 PSI air pressure @35 amps. During the initial cuts, he comments that the machine performs smoothly and cuts through material effectively.
He tests different materials, including mild steel tubing, thicker steel sections, and thin-wall aluminum, while adjusting amperage and air pressure depending on the application.
During thicker material tests, the review shows that travel speed plays an important role in achieving full penetration and cleaner cuts.
BULLI KID also tests creating holes in metal, similar to fabrication situations where a starting hole may be needed for components or modifications.
After adjusting settings, he is able to cut through thicker material without major issues.

Grid Cutting Test
The CUT-65DS PLUS includes a grid cutting mode designed for materials with changing cutting surfaces, where the arc moves between metal and open areas.
BULLI KID tests the machine on grid material to see how consistently it maintains the arc.
During the test, he notes:
- Smooth arc behavior
- Stable cutting performance
- No major interruptions
The review also shows that the machine maintains consistent operation even when the ground connection is placed on a painted surface.

Gouging Function Test
For the gouging test, BULLI KID changes the torch consumables to the gouging setup.
He explains that plasma gouging is useful for removing:
- Slag buildup
- Raised edges
- Excess material left after cutting
Unlike normal cutting, gouging removes material at an angle without fully cutting through the workpiece.
During testing, the gouging function helps remove buildup and prepares the surface for additional cleanup with grinding tools.

Marking Function Test
The marking function is one of the features BULLI KID finds most interesting.
Instead of creating a full cut, marking produces a lighter plasma arc that creates visible marks on the metal surface.
During the test, he uses the marking mode to create:
- Lines
- Layout marks
- Reference points
This can be useful when preparing fabrication work and identifying cutting locations before making the final cut.

Where the CUT-65DS PLUS Fits Best
Based on the testing shown in the video, the CUT-65DS PLUS is best suited for users who need a versatile plasma cutter for different fabrication tasks.
Potential applications include:
- Garage fabrication projects
- Metal repair work
- Custom metal fabrication
- Small-shop metalworking
- General cutting projects
- Surface preparation before welding
The strongest advantage shown in this review is versatility. Instead of using separate tools for cutting, gouging, and marking, the CUT-65DS PLUS combines multiple plasma functions in one machine.

Things to Keep in Mind
Although the review is positive, the video also shows that plasma cutting quality depends on proper setup and operator adjustment.
During testing, BULLI KID adjusts:
- Cutting amperage
- Air pressure
- Travel speed
- Material position
Some thicker material tests require additional adjustment to achieve full penetration.
Like any plasma cutter, final results depend on factors such as material thickness, air supply, consumable condition, and operator technique.
For high-volume industrial cutting or continuous production environments, a larger industrial plasma system may still be more suitable.
For hobbyists, fabricators, repair work, and small shops, the CUT-65DS PLUS provides a flexible option with multiple plasma functions in one machine.
Final Thoughts
BULLI KID's review provides a practical look at how the YesWelder CUT-65DS PLUS performs in shop-style cutting tasks.
Instead of only discussing specifications, the video demonstrates how the machine performs across different fabrication tasks, including standard cutting, material preparation, and layout work.
The review highlights the machine's simple setup, stable arc behavior, and ability to handle different metalworking applications with multiple plasma functions.
For users researching a portable plasma cutter for garage projects, repair work, and fabrication tasks, the CUT-65DS PLUS offers a combination of standard cutting capability and additional plasma functions in one compact machine.
Recommended Products