ER4043 5LB Aluminum TIG Welding Rod
ER4043 5LB Aluminum TIG Welding Rod


$36.00$45.00Save 20%
or 4 payments of $9.00 with Klarna
ER4043 is an AlSi5 aluminum TIG filler with approximately 5% silicon, improving weld-pool fluidity and reducing crack sensitivity on suitable wrought and cast aluminum.
ER4043 contains approximately 5% silicon, which improves weld-pool fluidity and reduces crack sensitivity when matched to a suitable aluminum base metal and welding procedure.
WARNING: This product can expose you to chemicals known to the State of California to cause cancer and birth defects or other reproductive harm. For more information, visit https://p65warnings.ca.gov.
Free standard shipping on orders over $150 within the contiguous US. Orders typically arrive in 3–5 business days. Expedited shipping options available at checkout.
Shipping policyShare your experience with other welders.
ER4043 5LB Aluminum TIG Welding Rod
Good product!
First time using a tig machine ( primeweld 225) and welding aluminum.... Watched a ton of videos and I'm very happy with the progress so far, these filler rods are great... I have stainless, alum and mild and all work great.
They were easy to learn with, I never had a problem.
These rods work just fine and are pretty clean out of the box. Why they make such short rods I don't know. I didn't mean to order short ones lol. I guess these are good for people doing a lot of 3 inch welds.
Wish they would use the same packaging as they do for their steel filler the box does not protect once opened.
I like that they are cut in half to fit into my tig rod holders.