Shopping Cart

Your cart looks a Little Empty!

Start your YesWelder journey with us

BEST SELLERS | FREE SHIPPING ON ALL ORDERS

Load image into Gallery viewer, Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Load image into Gallery viewer, Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Load image into Gallery viewer, Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Load image into Gallery viewer, Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Load image into Gallery viewer, Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Load image into Gallery viewer, Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes - YesWelder

Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes

Regular price
21.99
Sale price
21.99
Regular price
Sold out
Unit price
per 
  • VALUE
  • TOP QUALITY
  • HIGH COMPATIBLITY

Product Description

The Proper Selection and Preparation of Tungsten Electrodes

A welder's best friend, this ten pack of purple Rare Earth Mix TIG welding tungsten electrodes will help you get the job done.

Engineered to exact specifications, you can count on these long-lasting electrodes to perform during your most difficult welding application, time and time again.

With reliable arc-striking and a low burn-off rate, these electrodes maintain the highest quality of arc while adhering to ANSI and AWS standards.

The innovative Rare Earth Blend tungsten electrode contains 98.34% tungsten, 1.5% lanthanum, 0.08% Zirconium, 0.08% Yttrium, and is the perfect substitute for red thoriated electrodes. Sixty years of experience have culminated into these premium quality TIG welding tungsten electrodes, and you can benefit from that experience. Compare to E3 tungsten tig welding electrodes.

Specifications
  • Variant : 3/32"x7"(2.4x175mm)
  • SKU : WX-2.4
  • Weight : 188 g
  • Product Type : Hardware > Tool Accessories > Welding Accessories>Tungsten
  • Brand : YesWelder
  • Collection : Accessories Tungsten Electrodes
Shipping & Returns

Shipping
At YesWelder it’s our mission to provide quality welding equipment at genuinely affordable prices to welders everywhere. To do this, we work with manufacturers across the world and use a global distribution network to get you the goods for less.
Your equipment may be coming from the US, or Hong Kong, depending on the items. Your specific delivery date will depend on the dispatch country and delivery address.
When will I receive my order?
Most items are usually shipped within 3-5 working days.
We do recommend allowing up to 3 weeks for your order in peak times, such as a special offer or promotion. Delivery times are beyond our control but rest assured that we only work with reliable welding manufacturers and suppliers to give you the best service.
How do I track my order?
Your delivery confirmation email will contain your tracking number and order details.
Taxes and other charges
Depending on the country of delivery, you may be required to pay extra tax or charges such as VAT and/or import duties.
Returns Policy
We hope you love everything you purchase from YesWelder but if you’re not 100% happy, we want to know about it. Please get in touch with all feedback about our products so we can continue improving our service for you.
You can return any item within 30 days of purchase. If you wish to return a product, you must notify YesWelder within 7 days of receiving your item. Unfortunately due to logistics, we cannot accept return requests after this period.
All items being returned must be in new and resalable condition.
Refunds will be provided after the items have been received and inspected by YesWelder. A 10% stocking fee will be deducted from the total amount.
Shipping charges are non-refundable.
Taxes and any other charges incurred by the customer are non-refundable.

You may also like

Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes
Rare Earth Tungsten Electrode (Purple, EWG) | YesWelder TIG Welding Electrodes
-
+