YesWelder

Compare All Welders

TIG-205P-PRO Pulse TIG Welder Stick/DC TIG/Pulse TIG 3 In 1 TIG Welder

TIG-205P-PRO

Pulse DC TIG with stick backup and HF start.

From $249.00

or 4 payments of $62.25 with Klarna*

Learn more
TIG-200P-ACDC-PRO AC/DC Aluminum TIG Welder

TIG-200P-ACDC-PRO

AC/DC TIG built for aluminum, with pulse and HF start.

From $649.00

or 4 payments of $162.25 with Klarna*

Learn more
FIRSTESS CT2050 Powerful 7-in-1 Welder & Cutter

CT2050

7-in-1 AC/DC TIG, stick and plasma with a built-in air pump.

From $1,499.00

or 4 payments of $374.75 with Klarna*

Learn more

Quick Look

DC TIG pulse
Key Feature
LED
Display
Steel / Stainless
Material Compatibility
≤ 1/2" (13 mm) @ 220V
Recommended Thickness
200A
Max Output
TIG / Stick
Processes
110V / 220V
Input Voltage
AC/DC TIG for aluminum
Key Feature
LED
Display
Steel / Stainless / Aluminum
Material Compatibility
≤ 3/8" (10 mm) @ 220V
Recommended Thickness
200A
Max Output
TIG / Stick
Processes
110V / 220V
Input Voltage
Built-in pump + CNC
Key Feature
LED
Display
Steel / Stainless / Aluminum
Material Compatibility
≤ 1/4" (6 mm) @ 220V
Recommended Thickness
200A
Max Output
TIG / Stick / Plasma
Processes
96-265V
Input Voltage

Power & Output

Input Voltage

110V, 220V ±15% 50/60Hz

110V, 220V ±15% 50/60Hz

Single-phase 96-265V 50/60Hz

Processes

DC TIG (Pulse), Stick

AC/DC/MIX TIG (Pulse), Stick

AC/DC TIG (Pulse), Stick, Plasma (Built-in Pump)

Output Current Range

TIG: 10-160A @ 110V; 10-200A @ 220V Stick: 20-140A @ 110V; 20-160A @ 220V

TIG: 10-140A @ 110V; 10-200A @ 220V Stick: 20-120A @ 110V; 20-160A @ 220V

TIG: 5-160A @ 110V; 5-200A @ 220V Stick: 10-160A @ 110V; 10-200A @ 220V Plasma: 12-25A @ 110V; 12-45A @ 220V

Duty Cycle

TIG: 60% @ 200A

TIG: 30% @ 200A

TIG: 100% @ 200A

Detailed Duty Cycle

TIG (110V): 60% @ 160A; 100% @ 124A TIG (220V): 60% @ 200A; 100% @ 155A Stick (110V): 60% @ 140A; 100% @ 108A Stick (220V): 60% @ 160A; 100% @ 124A

TIG (110V): 60% @ 140A; 100% @ 108A TIG (220V): 30% @ 200A; 100% @ 110A Stick (110V): 60% @ 120A; 100% @ 93A Stick (220V): 30% @ 160A; 100% @ 88A

TIG (110V): 100% @ 160A TIG (220V): 100% @ 200A Stick (110V): 60% @ 120A; 100% @ 160A Stick (220V): 100% @ 160A Plasma (110V): 100% @ 25A Plasma (220V): 100% @ 45A

Material & Capability

Material Compatibility

TIG: Steel, Stainless Steel Stick: Steel

TIG: Steel, Stainless Steel, Aluminum Stick: Steel

TIG: Steel, Stainless Steel, Aluminum Stick: Steel Plasma: Steel, Stainless Steel, Aluminum

Recommended Thickness

TIG: ≤ 3/16" (5 mm) @ 110V; ≤ 1/2" (13 mm) @ 220V Stick: ≤ 1/4" (6 mm) @ 110V; ≤ 1/2" (13 mm) @ 220V

TIG: ≤ 5/16" (8 mm) @ 110V; ≤ 3/8" (10 mm) @ 220V Stick: ≤ 5/16" (8 mm) @ 110V; ≤ 3/8" (10 mm) @ 220V

TIG: ≤ 5/32" (4 mm) @ 110V; ≤ 3/16" (5 mm) @ 220V Stick: ≤ 3/16" (5 mm) @ 110V; ≤ 1/4" (6 mm) @ 220V

Clean Cut Thickness

Not applicable

Not applicable

3/8" (10 mm) @ 110V 19/32" (15 mm) @ 220V

Severance Cut Thickness

Not applicable

Not applicable

3/4" (20 mm) @ 110V 1 3/16" (30 mm) @ 220V

TIG

TIG Ignition Type

HF Start

HF Start

HF Start

Foot Pedal Compatibility

Supported

Supported

Supported

Tungsten Type

WT20, WC20, WL20, WL15

WT20, WC20, WL20, WL15, WP

WT20, WC20, WL20, WL15, WP

Tungsten Diameter

≤ 5/32" (4.0 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V

≤ 5/32" (4.0 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V

≤ 5/32" (4.0 mm)

TIG Torch Type

WP-17 (M16 × 1.5 connector, 5-pin control cable)

WP-26 (M16 × 1.5 connector, 5-pin control cable)

WP-26 (M16 × 1.5 gas connector, KDP35-50 electric connector, 5-pin control cable)

TIG Filler Rod Material

ER70S-6, ER308L

ER70S-6, ER308L, ER4043

ER70S-6, ER308L, ER4043

TIG Filler Rod Diameter

≤ 1/8" (3.2 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V

≤ 1/8" (3.2 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V

≤ 3/32" (2.4 mm) @ 110V ≤ 1/8" (3.2 mm) @ 220V

Gas Requirements

100% Argon

100% Argon

100% Argon

Consumables Compatibility

WP-17 / WP-18 / WP-26

WP-17 / WP-18 / WP-26

WP-17 / WP-18 / WP-26

Stick

Stick Electrode Type

E6011 / E6013 / E7018

E6010 / E6011 / E6013 / E7018

E6010 / E6011 / E6013 / E7018

Stick Electrode Diameter

≤ 3/32" (2.4 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V

≤ 3/32" (2.4 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V

≤ 3/32" (2.4 mm) @ 110V ≤ 5/32" (4.0 mm) @ 220V

Plasma Cutting

Pilot Arc

Not applicable

Not applicable

Supported

Plasma Arc Starting

Not applicable

Not applicable

Back-flow Start

Air Pressure

Not applicable

Not applicable

45-60 PSI @ 110V; 55-75 PSI @ 220V

Air Flow

Not applicable

Not applicable

≥ 6.0 CFM

Recommended Compressor

Not applicable

Not applicable

30-60 gal, ≥ 2 HP

Plasma Torch Type

Not applicable

Not applicable

IPL50 (M16 × 1.5 connector, 5-pin control cable)

CNC Capability

Not supported

Not supported

CNC ready

Gas Requirements

Not applicable

Not applicable

Compressed Air

Consumables Compatibility

Not applicable

Not applicable

IPL50-45

Physical & Safety

Display

LED

LED

LED

Fan Control

Continuous Fan Mode

Fan on Demand

Fan on Demand

App Control

Not supported

Not supported

Not supported

Weight

10.7 lbs

19.59 lbs

44.9 lbs

Dimensions

13.98" × 6.1" × 9.45"

15.7" × 7.09" × 9.84"

18.5" × 13.6" × 8.7"

Protection Features

Overheat Overcurrent Overvoltage

Overheat

Overheat Overcurrent VRD (Voltage Reduction Device) - Stick

General

Input Current

50A @ 110V; 40A @ 220V

50A @ 110V; 40A @ 220V

50A @ 110V; 40A @ 220V

Open Circuit Voltage (OCV)

TIG/Stick: 65V

TIG/Stick: 75V

TIG: 68V Stick: 68V (VRD: 7V) Plasma: 312V

Generator Compatibility

Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.

Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.

Generator not recommended. If necessary, use at least a 10 kW (15 HP), 120/240V generator with AVR.

Cable Length

Ground: 10 ft (3 m) TIG Torch: 13 ft (4 m)

Ground: 10 ft (3 m) TIG Torch: 13 ft (4 m)

Ground: 10 ft (3 m) TIG Torch: 13 ft (4 m) Plasma Torch: 13 ft (4 m)

Power Cord Length

6.5 ft (2 m)

6.5 ft (2 m)

6.5 ft (2 m)

Certification

CE, ETL, UL

CE, ETL, UL

Not applicable

Warranty

2 Years

2 Years

3 Year

*Financing available to qualified customers through Klarna. Pay-in-4 and monthly options are subject to eligibility and approval; see checkout for available plans and terms. Prices shown are starting prices for each model and may vary by configuration.