The jacket uses 11 oz (310 g) FR cotton with a button front, adjustable cuffs and covered chest and sleeve pockets. The manufacturer states compliance with NFPA 2112.
Material and Construction
- Material: 11 oz (310 g) FR cotton
- Manufacturer-stated standard: NFPA 2112
- Stand collar, button closure and adjustable cuffs
- Covered chest pocket and sleeve pocket
- Color: Black
Size Guide
| Size | Neck | Chest Width | Sleeve | Shoulder Width | Length |
|---|---|---|---|---|---|
| M | 20.5" (52.1 cm) | 23.6" (59.9 cm) | 24.8" (63 cm) | 19.3" (49 cm) | 29.5" (74.9 cm) |
| L | 20.5" (52.1 cm) | 24.6" (62.5 cm) | 25.6" (65 cm) | 19.8" (50.3 cm) | 30" (76.2 cm) |
| XL | 20.9" (53.1 cm) | 25.6" (65 cm) | 26.4" (67.1 cm) | 20.4" (51.8 cm) | 30.5" (77.5 cm) |
| XXL | 20.9" (53.1 cm) | 26.6" (67.6 cm) | 27.2" (69.1 cm) | 20.9" (53.1 cm) | 30.9" (78.5 cm) |
| XXXL | 21.3" (54.1 cm) | 27.6" (70.1 cm) | 27.9" (70.9 cm) | 21.5" (54.6 cm) | 31.4" (79.8 cm) |
Manual measurements may vary by approximately 0.4" (1 cm). Use these garment measurements as a reference and allow room for underlayers.
Care and PPE Selection
Dry cleaning is recommended. If laundering is permitted by the sewn care label, do not exceed . Inspect the garment before use and select the complete PPE system according to the welding and workplace hazards.