E308LFC-O Stainless Flux-Cored MIG Wire

Vendor
YesWelder
Regular price
31.00
Sale price
31.00

E308LFC-O is a self-shielded stainless flux-cored wire for repair and light fabrication on compatible 304/304L, 308/308L, 321, and 347 stainless steels. It requires no external shielding gas and supports flat, horizontal, vertical, and overhead welding.

Materials and Applications

  • 304 and 304L stainless steel
  • 308 and 308L stainless steel
  • 321 and 347 stainless steel
  • Outdoor stainless repair, maintenance, and light fabrication

Key Specifications

  • Classification: E308LFC-O
  • Process: Flux-Cored
  • Shielding gas: Not required
  • Spool weight: 2 lb (0.9 kg)
  • Diameter options: .030" (0.8 mm) and .035" (0.9 mm)
  • Welding positions: Flat, horizontal, vertical, and overhead