ER70S-6/10LB 10LB Spool Carbon Steel Solid MIG Welding Wire

Vendor
YesWelder
Regular price
42.00
Sale price
42.00

ER70S-6 is a copper-coated mild steel MIG wire with high manganese and silicon content, designed for strong arc stability and excellent performance on rusty or dirty steel. It works well with 100% CO₂ or Ar/CO₂ shielding gas and produces smooth welds with minimal spatter.

Key Features

  • High Mn & Si for better tolerance on dirty/rusty steel
  • Smooth arc and stable wire feeding
  • Works with CO₂ or Ar/CO₂ gas
  • Low spatter, clean weld finish
  • Suitable for single and multi-pass welding

Applications

  • Structural and construction welding
  • Automotive and truck repair
  • Farm equipment and maintenance
  • General steel fabrication
  • Rusty or poor fit-up materials

Materials Compatibility

Mild Steel
Carbon Steel
Low-Alloy Steel

Specifications

  • Wire Type: ER70S-6
  • Diameter: 0.8mm / 0.9mm
  • Material: Copper-coated mild steel
  • Gas: CO₂ / Ar-CO₂ mix
  • Spool: 10 lb (4.5 kg)


Package Includes

1 × ER70S-6 MIG Wire Spool (10 lb)

FAQ

Q: Does it require gas?
Yes, it must be used with shielding gas.

Q: Can it weld rusty steel?
Yes, it is designed for surfaces with rust, oil, or dirt.

Q: What machines is it compatible with?
Most MIG welders supporting 0.8mm / 0.9mm wire and 10 lb spools.