WL15 (EWLa-1.5) is a gold-tip 1.5% lanthanated tungsten that balances arc starting, arc control and electrode life across AC and DC TIG welding.
Why Choose WL15
WL15 offers a practical balance of arc starting, arc control and electrode life across AC and DC TIG applications. The lanthanated composition is non-radioactive and works well for both precision jobs and everyday fabrication.
Key Specifications
- Classification: WL15 / EWLa-1.5
- Composition: 1.5% lanthanated tungsten
- Current: AC or DC
- Color code: Gold
- Length: 7"(175 mm)
- Package: 10 electrodes, vacuum sealed
- Diameter options: .040" (1.0 mm), 1/16" (1.6 mm), 3/32" (2.4 mm), and 1/8" (3.2 mm)