BWX-01 provides adjustable heated storage for compatible covered electrodes in the shop or field. Its 110V input and 85°F to 300°F temperature range support holding requirements that vary by electrode classification and manufacturer.
Heated Electrode Storage
Use the oven to hold compatible covered electrodes under controlled heat and reduce moisture pickup during storage. Electrode storage and reconditioning requirements vary by classification and manufacturer, so follow the instructions supplied with the electrodes.
Capacity Comparison
- 15 lb (6.8 kg) model: Holds electrodes up to 14" (356 mm)
- 24 lb (10.9 kg) model: Holds electrodes up to 17" (432 mm)
Key Specifications
- Input: 110V AC
- Temperature range: 85-300°F (29-149°C)
- Included: Oven, power cord and user manual